DEGRADATION OF POLYMETHYLMETHACRYLATE IN SUPERCRITICAL TOLUENE AND TETRAHYDROFURAN

Title
DEGRADATION OF POLYMETHYLMETHACRYLATE IN SUPERCRITICAL TOLUENE AND TETRAHYDROFURAN
Author
배성열
Issue Date
2004-02
Publisher
World Scientific
Citation
Frontiers on Separation Science and Technology, Page. 142-146
Abstract
With increasing plastic consumption, its recycling is becoming a major environmental concern. Provided that polymer can be broken down into useful low molecular-weight material, plastic waste can be used as a highly valuable feedstock. The degradation of polymethylmethacrylate (PMMA) in supercritical Toluene was carried out in stainless steel autoclave reactor at temperature of 360-480°C, pressure of 52-70 bar. In case of PMMA in supercritical Tetrahydrofuran (THF), it was carried out in the same reactor at temperature of 360-480°C, pressure of 65-105 bar. Each product was analyzed by GC(FID) and GC/MS. It was found that the weight selectivity of product was influenced by temperature, pressure. It could be controlled by varying these reaction conditions.
URI
https://repository.hanyang.ac.kr/handle/20.500.11754/132078https://www.worldscientific.com/doi/abs/10.1142/9789812702623_0029
ISBN
978-981-238-916-9; 978-981-4482-33-2
DOI
10.1142/9789812702623_0029
Appears in Collections:
COLLEGE OF ENGINEERING SCIENCES[E](공학대학) > MATERIALS SCIENCE AND CHEMICAL ENGINEERING(재료화학공학과) > Articles
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML


qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE