2016-06 | Factors Affecting the Inclusion Potency for Acicular Ferrite Nucleation in High-Strength Steel Welds | 이창희 |
2011-03 | Fatigue crack growth behavior of the simulated HAZ of 800 MPa grade high-performance steel | 이창희 |
2016-03 | Formation and heat treatment of kinetic sprayed nanocrystalline Al coatings reinforced with multi-walled carbon nanotubes: The relationship between microstructural features and physical properties | 이창희 |
2011-01 | Formation of coating and tribological behavior of kinetic sprayed Fe-based bulk metallic glass | 이창희 |
2015-05 | Formation of Mn-depleted zone in Ti-containing weld metals | 이창희 |
2019-03 | Formation of Secondary Phases and Their Effect on the Mechanical Properties of Joints Formed by TLP Bonding Using Fe-B-Si Insert Metal in Duplex Stainless Steel | 이창희 |
2020-05 | Fusion Weldabilities of Advanced High Manganese Steels: A Review | 이창희 |
2013-06 | Hot Cracking Susceptibility of Fe-Mn-Al-C Austenitic Steel Welds | 이창희 |
2017-01 | Hot deformation behavior and microstructural evolution of alumina-forming austenitic heat-resistant steels during hot compression | 이창희 |
2016-12 | Hot ductility and hot cracking susceptibility of Ti-modified austenitic high Mn steel weld HAZ | 이창희 |
2011-06 | Hydrogen Dissolution in the TiO(2)-SiO(2)-FeO and TiO(2)-SiO(2)-MnO Based Welding-Type Fluxes | 이창희 |
2019-09 | The importance of intimate inter-crystallite bonding for the plasma erosion resistance of vacuum kinetic sprayed Y2O3 coating | 이창희 |
2017-06 | Improved creep strength of alumina-forming austenitic heat-resistant steels through W addition | 이창희 |
2018-03 | Improvement of circumferential ductility by reducing discontinuities in a high-Mn TWIP steel weldment | 이창희 |
2018-12 | In Situ Investigation of Intergranular Stress Corrosion Cracking Initiation and Coalescence and Effects of Geometric and Microstructural Characteristics | 이창희 |
2011-04 | Inclusions Nucleating Intragranular Polygonal Ferrite and Acicular Ferrite in Low Alloyed Carbon Manganese Steel Welds | 이창희 |
2017-10 | Inflight Particle Behavior in the Vacuum Kinetic Spray Process | 이창희 |
2019-06 | Influence of alloying elements in low transformation temperature filler alloys on microstructure and mechanical properties | 이창희 |
2015-01 | Influence of Cr on Weld Solidification Cracking in Fe-15Mn-0.5C-3.5Al-xCr Alloys | 이창희 |
2018-05 | Influence of kappa-carbide precipitation on the microstructure and mechanical properties in the weld heat-affected zone in various FeMnAlC alloys | 이창희 |
2013-02 | Influence of Oxygen Content on Microstructure and Inclusion Characteristics of Bainitic Weld Metals | 이창희 |
2018-03 | Influence of Si on sigma phase precipitation and pitting corrosion in superaustenitic stainless steel weld metal | 이창희 |
2016-10 | Influence of substrate roughness on bonding mechanism in cold spray | 이창희 |
2011-04 | Influence of the Interface Temperature and Strain Gradients on the Impact Energy Model of a Soft Particle on a Hard Substrate during Kinetic Spraying | 이창희 |
2014-01 | Influence of Ti on non-metallic inclusion formation and acicular ferrite nucleation in high-strength low-alloy steel weld metals | 이창희 |
2012-06 | Interfacial bonding and microstructural evolution of Al in kinetic spraying | 이창희 |
2018-04 | Investigations of the microstructure evolution and tensile deformation behavior of austenitic Fe-Mn-Al-C lightweight steels and the effect of Mo addition | 이창희 |
2016-02 | Kinetic Spraying Deposition of Reactive-Enhanced Al-Ni Composite for Shaped Charge Liner Applications | 이창희 |
2012-04 | Liquation behavior in the weld HAZ of high Si nodular iron | 이창희 |
2019-12 | Local -brittle cracking in the heat-affected zone of lightweight steels | 이창희 |