dc.description.abstractIn 3-dimensional memories such as NAND flash and cross-point memory, the integration fabrication processes face a notable initial-step-height of an isolated SiO2-film deposition, which is an extremely critical process removing such initial-step-height perfectly via chemical mechanical planarization (CMP). The SiO2-film polishing-rate difference was generated between upper and lower locations of initial-step-height and was evidently depended on the nano-ceria abrasive size in an isolated SiO2-film CMP slurry; that is, the polishing ratio of the upper location to lower location remarkably increased from 4.5:1 to 11.5:1, as the ceria abrasive size increased from 21.3 to 81.0 nm. The difference of polishing rate was associated with a local pressure difference between upper and lower locations of initial-step-height; that is, the local pressure at the upper location remarkably increased from 5.2 to 14.2 PSI, while it at the lower location very slightly decreased from 1.0 to 1.3 PSI, as the ceria abrasive size increase from 21.3 to 81.0 nm. Thus, a larger ceria abrasive size in an isolated SiO2-film CMP slurry led to better removal ability (i.e., a shorter polishing time of initial-step-height and a thicker remaining isolated SiO2-film thickness).en_US
dc.description.sponsorshipThis work was supported by the Republic of Korea's MOTIE (Ministry of Trade, Industry and Energy) (10085643) and KSRC (Korea Semiconductor Research Consortium) support program for the development of future semiconductor devices, by the Brain Korea 21 PLUS Program and the Samsung Electronics' University R&D program, Samsung Display Co. Ltd.en_US
dc.language.isoenen_US
dc.publisherKOREAN PHYSICAL SOCen_US
dc.subjectCMP; CMP slurry; Isolated SiO2-flm; Initial step height; Ceria abrasive sizeen_US
dc.titleImpact of wet ceria abrasive size on initial step height removal efficiency for Isolated SiO2 film chemical mechanical planarizationen_US
dc.typeArticleen_US
dc.relation.no1-
dc.relation.volume78-
dc.identifier.doi10.1007/s40042-020-00022-wen_US
dc.relation.page51-57-
dc.relation.journalJOURNAL OF THE KOREAN PHYSICAL SOCIETY-
dc.contributor.googleauthorYun, Sang-Su-
dc.contributor.googleauthorPark, Jea-Gun-
dc.relation.code2020048704-
dc.sector.campusS-
dc.sector.daehakCOLLEGE OF ENGINEERING[S]-
dc.sector.departmentSCHOOL OF ELECTRONIC ENGINEERING-
dc.identifier.pidparkjgl-
dc.identifier.orcidhttps://orcid.org/0000-0002-5831-2854-
Appears in Collections:
COLLEGE OF ENGINEERING[S](공과대학) > ELECTRONIC ENGINEERING(융합전자공학부) > Articles
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML


qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE