2012-10 | Behavior of Cu precipitates during thermo-mechanical cycling in the weld CGHAZ of Cu-containing HSLA steel | 이창희 |
2020-07 | Bonding formation in vacuum kinetic-sprayed Y2O3 particles induced by high-velocity impact | 이창희 |
2014-06 | Bonding, Reactivity, and Mechanical Properties of the Kinetic-Sprayed Deposition of Al for a Thermally Activated Reactive Cu Liner | 이창희 |
2013-01 | Characteristics of inclusions in rutile-type FCAW weld metal | 이창희 |
2018-07 | Characteristics of kinetic sprayed Ta in terms of the deposition behavior, microstructural evolution and mechanical properties: Effect of strain-rate-dependent response of Ta at high temperature | 이창희 |
2016-08 | Characterization of bond line discontinuities in a high-Mn TWIP steel pipe welded by HF-ERW | 이창희 |
2015-08 | Characterization of Inclusions Formed in Ti-containing Steel Weld Metals | 이창희 |
2019-03 | Characterization of Mechanical and Metallurgical Notch Effects of DP980 Steel Weld Joints in Fatigue Performance | 이창희 |
2012-12 | Cold cracking susceptibility of boron added high-strength bainitic steels | 이창희 |
2019-04 | A comparison of cross-tension properties and fracture behavior between similar and dissimilar resistance spot-weldments in medium-Mn TRIP steel | 이창희 |
2019-12 | Computational Research on Factors Affecting Particle Velocity in a Vacuum Kinetic Spray Process | 이창희 |
2019-03 | Consideration of the criteria for successful deposition in cermet kinetic spraying using WC-17Co powder | 이창희 |
2018-01 | Correlation Between Microstructure and Low-Temperature Impact Toughness of Simulated Reheated Zones in the Multi-pass Weld Metal of High-Strength Steel | 이창희 |
2014-07 | Correlation between microstructure and mechanical properties of heat affected zones in Fe-8Mn-0.06C steel welds | 이창희 |
2017-02 | Correlation of Fracture Mode Transition of Ceramic Particle with Critical Velocity for Successful Deposition in Vacuum Kinetic Spraying Process | 이창희 |
2016-12 | Correlation of microstructure with tribological properties in atmospheric plasma sprayed Mo-added ferrous coating | 이창희 |
2012-05 | Correlation of particle impact conditions with bonding, nanocrystal formation and mechanical properties in kinetic sprayed nickel | 이창희 |
2020-03 | Correlation of Plasma Erosion Resistance and the Microstructure of YF3 Coatings Prepared by Vacuum Kinetic Spray | 이창희 |
2013-01 | Corrosion fatigue behaviors of HSB800 and its HAZs in air and seawater environments | 이창희 |
2011-06 | Dependence of Bonding Mechanisms of Cold Sprayed Coatings on Strain-Rate-Induced Non-Equilibrium Phase Transformation | 이창희 |
2013-07 | Deposition Behavior and Microstructural Features of Vacuum Kinetic Sprayed Aluminum Nitride | 이창희 |
2012-05 | Deposition Behaviors and Microstructural Features of Vacuum Kinetic Sprayed AlN | 이창희 |
2015-02 | Deposition of Workability-Enhancing Disposable Thick Fe Deposits on Fe-Si Alloy Sheets Using Thermal and Kinetic Spray Processes | 이창희 |
2013-11 | Different aspect of pitting corrosion and interphase corrosion in the weld heat-affected zone of high-nitrogen Fe-18Cr-10Mn-N steel | 이창희 |
2015-11 | Dynamic fragmentation process and fragment microstructure evolution of alumina particles in a vacuum kinetic spraying system | 이창희 |
2012-12 | Effect of Complex Inclusion Particles on the Solidification Structure of Fe-Ni-Mn-Mo Alloy | 이창희 |
2017-01 | Effect of Dilution on Wear Performance of Plasma Transferred Arc Deposited Layers | 이창희 |
2011-09 | The effect of fracture induced ceramic free surfaces for vacuum kinetic spray bonding | 이창희 |
2014-12 | Effect of gas flow rate on deposition behavior of Fe-based amorphous alloys in vacuum kinetic spray process | 이창희 |
2016-09 | Effect of intermetallic compounds on the bonding state of kinetic sprayed Al deposit on Cu after heat-treatment | 이창희 |