2011-08 | Microstructural Characterization of Clad Interface in Welds of Ni-Cr-Mo High Strength Low Alloy Steel | 이창희 |
2015-01 | Microstructural evolution and solidification cracking susceptibility of Fe-18Mn-0.6C-xAl steel welds | 이창희 |
2019-04 | Microstructural evolution of laser-brazed joint of Mg2Si and HMS on DBC substrate for thermoelectric generator | 이창희 |
2017-12 | Microstructural features affecting optical properties of vacuum kinetic sprayed Al2O3 thin film | 이창희 |
2012-02 | Microstructure and texture of Al coating during kinetic spraying and heat treatment | 이창희 |
2018-03 | Microstructure control to improve creep strength of alumina-forming austenitic heat-resistant steel by pre-strain | 이창희 |
2017-10 | Microstructure Evolution and Age-Hardening Behavior of Microalloyed Austenitic Fe-30Mn-9Al-0.9C Light-Weight Steels | 이창희 |
2013-01 | Microstructure Evolution of Titanium Nitride Film during Vacuum Kinetic Spraying | 이창희 |
2015-04 | Microstructure of Kinetic Spray Coatings: A Review | 이창희 |
2014-09 | Mn-Depleted Zone Formation in Rapidly Cooled High-Strength Low-Alloy Steel Welds | 이창희 |
2012-12 | Nanoscale deformation twinning at ultrahigh strain rates during kinetic spraying of nickel | 이창희 |
2020-07 | A new class of lightweight, stainless steels with ultra-high strength and large ductility | 이창희 |
2014-04 | Oxide Formation Mechanisms in High Manganese Steel Welds | 이창희 |
2019-02 | Performance Comparison of Double-Layer Liner for Shaped Charge Fabricated Using Kinetic Spray | 이창희 |
2012-12 | Pinning efficiency of austenite grain boundary by a cubic shaped TiN particle in hot rolled HSLA steel | 이창희 |
2018-08 | Possibility of Mn substitution of Ni through evaluation of mechanical properties and corrosion resistance in superaustenitic stainless steel weld metal | 이창희 |
2012-02 | Post-weld heat treatment cracking susceptibility of T23 weld metals for fossil fuel applications | 이창희 |
2019-01 | Precipitation behavior and its effect on mechanical properties in weld heat-affected zone in age hardened FeMnAlC lightweight steels | 이창희 |
2018-10 | Precipitation behavior of the sigma phase with Ni and Mn content variations in superaustenitic stainless steel weld metal | 이창희 |
2020-05 | Promotion of the fragmentation and densification for a dense vacuum kinetic-sprayed Y2O3 coating by heat-treatment of feedstock powder | 이창희 |
2019-06 | Quantitative Evaluation of Nucleation Potency of Ti-containing Inclusions for Acicular Ferrite | 이창희 |
2020-07 | Reactivity Enhancement and Fabrication of Al-MoO3 Thermite coating using ball milling for kinetic spraying | 이창희 |
2019-10 | Remarkable improvement in resistance spot weldability of medium-Mn TRIP steel by paint-baking heat treatment | 이창희 |
2015-08 | Residual stress and crack initiation in laser clad composite layer with Co-based alloy and WC plus NiCr | 이창희 |
2013-03 | Restoration of face-centered cubic metals subjected to kinetic spraying | 이창희 |
2013-02 | Role of Ca treatment in hydrogen induced cracking of hot rolled API pipeline steel in acid sour media | 이창희 |
2017-01 | The role of phosphorus in precipitation behavior and its effect on the creep properties of alumina-forming austenitic heat-resistant steels | 이창희 |
2015-11 | Role of spray processes on microstructural evolution, and physical and mechanical properties of multi-walled carbon nanotube reinforced cu composite coatings | 이창희 |
2019-07 | Roles of (Fe, Mn)(3)Al Precipitates and MBIP on the Hot Ductility Behavior of Fe-30Mn-9Al-0.9C Lightweight Steels | 이창희 |
2018-06 | Roles of Particle Size Distribution in Bimodal Feedstocks on the Deposition Behavior and Film Properties in Vacuum Kinetic Spraying | 이창희 |