251 0

Role of air pollutant for deterioration of Taj Mahal by identifying corrosion products on surface of metals

Title
Role of air pollutant for deterioration of Taj Mahal by identifying corrosion products on surface of metals
Author
지텐드라 쿠마 싱
Keywords
Taj Mahal; India; Air pollution; Metal corrosion; Electrochemical impedance spectroscopy; X-ray difraction; Raman spectroscopy
Issue Date
2021-08
Publisher
SPRINGER
Citation
INTERNATIONAL JOURNAL OF ENVIRONMENTAL SCIENCE AND TECHNOLOGY, v. 19, NO 2, Page. 829-838
Abstract
Deterioration of metallic and non-metallic structures and monuments is largely controlled by their surrounding environment. The Taj Mahal, a UNESCO (United Nations Educational, Scientific and Cultural Organization) world heritage situated in Agra of India built in seventeenth century using white marbles, is famous for its aesthetic look. Gradual yellowing and blackening of the monument are matter of great concern, and if not controlled, the heritage structure may lose its glaze and beauty. Extensive studies available on deteriorating effect of the monument miss a vital point related to the pollutants coming from severely polluted River Yamuna which flows very close to the Taj Mahal. To ascertain the possible effects of the pollutants carbon steel, copper and zinc samples were exposed for four years at the premise of Taj Mahal. The surface characterization of the exposed metals with electrochemical impedance spectroscopy, Raman spectroscopy and X-ray diffraction reveals the formation of respective sulphides of the studied metals. The findings suggest that the hydrogen sulphide from the polluted Yamuna River had damaging effect. The wind rose diagram developed at site of exposure further supports the above findings. The corrosion rate of copper was found to be 2.46 mu m/year. This observation as well as identification of corrosion products formed on the metal surface (strong peaks of copper sulphide) provided strong evidences that the hydrogen sulphide evolved from the polluted river accelerated the deterioration of the metal.
URI
https://link.springer.com/article/10.1007/s13762-021-03613-7https://repository.hanyang.ac.kr/handle/20.500.11754/172457
ISSN
17351472; 17352630
DOI
10.1007/s13762-021-03613-7
Appears in Collections:
OFFICE OF ACADEMIC AFFAIRS[E](교무처) > Center for Creative Convergence Education(창의융합교육원) > Articles
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML


qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE