dc.identifier.citationJOURNAL OF THE ELECTROCHEMICAL SOCIETY, v. 158, NO 4, Page. 394-400en_US
dc.identifier.issn0013-4651-
dc.identifier.urihttp://jes.ecsdl.org/content/158/4/H394.short-
dc.description.abstractThe generation of pad debris during the chemical mechanical planarization (CMP) process was studied. A fresh pad was conditioned with deionized water alone without polishing any wafer in order to characterize the pad debris exclusively. It was found that the pad debris presented in several size ranges with irregular shapes, mostly in agglomerated form. Polishing experiments were performed continuously without conditioning the pad, and the byproducts were gathered several times during the process. No pad debris was found in the gathered slurry during this process, but dispersion of some agglomerated silica particles was observed. The slurry was gathered during CMP processes conducted under both in situ and ex situ pad conditions. The generation of pad debris during polishing was observed with in situ conditioning but not observed with ex situ conditioning. The effect of the presence of pad debris on scratch formation was also studied, and it was found that the occurrence of pad debris seriously increased the number of scratches. An increase in the number of diamonds per unit area of a conditioner could ultimately avoid the generation of pad debris, eventually reducing the scratch formation by sustaining the same removal rate and nonuniformity after the CMP process. (C) 2011 The Electrochemical Society. [DOI: 10.1149/1.3551507] All rights reserved.en_US
dc.description.sponsorshipThis research was supported by Basic Science Research Program through the National Research Foundation of Korea (NRF) funded by the Ministry of Education, Science and Technology (#R11-2008-044-02004-0).en_US
dc.language.isoenen_US
dc.publisherELECTROCHEMICAL SOC INCen_US
dc.subjectCHEMICAL-MECHANICAL PLANARIZATIONen_US
dc.subjectMICRO JET TECHNOLOGYen_US
dc.subjectSURFACE CHARACTERIZATIONen_US
dc.subjectSLURRY FILTERen_US
dc.subjectCOPPER CMPen_US
dc.subjectSILICAen_US
dc.subjectREDUCTIONen_US
dc.subjectREMOVALen_US
dc.subjectDIAMONDen_US
dc.subjectSIO2-FILMSen_US
dc.titleGeneration of Pad Debris during Oxide CMP Process and Its Role in Scratch Formationen_US
dc.typeArticleen_US
dc.relation.no4-
dc.relation.volume158-
dc.identifier.doi10.1149/1.3551507-
dc.relation.page394-400-
dc.relation.journalJOURNAL OF THE ELECTROCHEMICAL SOCIETY-
dc.contributor.googleauthorPrasad, Y. Nagendra-
dc.contributor.googleauthorKwon, Tae-Young-
dc.contributor.googleauthorKim, In-Kwon-
dc.contributor.googleauthorKim, In-Gon-
dc.contributor.googleauthorPark, Jin-Goo-
dc.relation.code2011205950-
dc.sector.campusS-
dc.sector.daehakGRADUATE SCHOOL[S]-
dc.sector.departmentDEPARTMENT OF BIONANOTECHNOLOGY-
dc.identifier.pidjgpark-
Appears in Collections:
GRADUATE SCHOOL[S](대학원) > BIONANOTECHNOLOGY(바이오나노학과) > Articles
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML


qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE