294 197

Mechanical Degradation and Thermal Decomposition of Ethylene-Vinyl Acetate (EVA) Polymer-Modified Cement Mortar (PCM) Exposed to High-Temperature

Title
Mechanical Degradation and Thermal Decomposition of Ethylene-Vinyl Acetate (EVA) Polymer-Modified Cement Mortar (PCM) Exposed to High-Temperature
Author
배성철
Keywords
polymer-modified cement mortar; ethylene-vinyl acetate; mechanical properties; repair materials; heating
Issue Date
2019-01
Publisher
MDPI
Citation
SUSTAINABILITY, v. 11, Issue2, NO. 500
Abstract
A polymer-modified cement mortar (PCM) is widely used as a repair material for reinforced concrete (RC) structures owing to its excellent strength and durability. However, considering the maintenance of the RC structures and the use period of the structures, the change in the physical properties of the PCM should be evaluated when exposed to various high-temperature environments, such as fires. In this study, the degradation of the mechanical properties (compressive strength and modulus of elasticity), thermal decomposition of the PCM in various high-temperature environments, and the change in the pore structure of the PCM after exposure to high temperatures were quantitatively investigated. A mechanical property evaluation of PCM was performed under three heating conditions: (i) heating in a compression tester, (ii) heating the specimen in an oven to a predetermined temperature and then moving it to a compression tester preheated to the same temperature, and (iii) cooling to room temperature after heating. In the experiment, a PCM specimen was prepared by changing the polymer-cement ratio (polymer content) of ethylene-vinyl acetate (EVA), the most commonly used polymer, to perform a high-temperature sectional test from 200 to 800 degrees C. In addition, to investigate the change in the PCM mechanical properties in the high-temperature region, in terms of the pyrolysis of EVA, the porosity change and mass change were examined using thermal analysis and mercury intrusion porosimetry. Before heating, the compressive strength of the PCM increased with the EVA content up to 10 % of the polymer-cement ratio. Under the cooling conditions after heating up to 200 degrees C, the mechanical performance of the PCM was restored, whereas the degradation of the mechanical properties of the PCM without cooling was more pronounced. Furthermore, the mass loss, heat flow, and the total porosity of the PCM increased as the EVA content increased, which is correlated with the degradation of the mechanical properties of the PCM.
URI
https://www.mdpi.com/2071-1050/11/2/500https://repository.hanyang.ac.kr/handle/20.500.11754/102822
ISSN
2071-1050
DOI
10.3390/su11020500
Appears in Collections:
COLLEGE OF ENGINEERING[S](공과대학) > ARCHITECTURAL ENGINEERING(건축공학부) > Articles
Files in This Item:
Mechanical Degradation and Thermal Decomposition of Ethylene-Vinyl Acetate (EVA) Polymer-Modified Cement Mortar (PCM) Exposed to High-Temperature.pdfDownload
Export
RIS (EndNote)
XLS (Excel)
XML


qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE